Abstract:
The use of high pressure ($\sim$8 GPa) in the formation of composite quasi-crystalline materials from powders made it possible to create practically poreless samples with a density close to the maximum known for this type of quasi-crystals. For samples with a nickel binder, sintered at a temperature of 550$^\circ$C, a very low coefficient of friction was obtained, which retain its value during the testing.