Abstract:
A method for reducing thermooptic deformations of the active element in a laser with an LiF crystal containing F2– color centers was proposed and implemented. Continuous-wave emission was achieved at λ = 1.1–1.2 μm at T = 313 K. The output power was 6 mW when the pump power was 3 W.