  1. Experimental research of residual stresses kinetics in the hardened hollow cylindrical specimens of D16T alloy at the axial tension under the creep conditions

    Vestn. Samar. Gos. Tekhn. Univ., Ser. Fiz.-Mat. Nauki [J. Samara State Tech. Univ., Ser. Phys. Math. Sci.], 20:2 (2016),  290–305
  2. Influence of air shot blasting and temperature exposure on residual stresses and fatigue strength of notched specimens from alloys V95 and D16T

    Vestn. Samar. Gos. Tekhn. Univ., Ser. Fiz.-Mat. Nauki [J. Samara State Tech. Univ., Ser. Phys. Math. Sci.], 3(24) (2011),  181–184
  3. Прогнозирование предела выносливости корсетных образцов из сплава ВКС-5 по остаточным напряжениям

    Matem. Mod. Kraev. Zadachi, 1 (2010),  311–314
  4. Прогнозирование предела выносливости образцов из сплава ЭИ698ВД при упрочнении стальными микрошариками

    Matem. Mod. Kraev. Zadachi, 1 (2010),  308–311
  5. Учёт влияния теоретического коэффициента концентрации напряжений на предел выносливости упрочнённой детали

    Matem. Mod. Kraev. Zadachi, 1 (2010),  184–186
  6. Остаточные напряжения и предел выносливости образцов с надрезами из сплавов В95 и Д16Т после пневмодробеструйной обработки

    Matem. Mod. Kraev. Zadachi, 1 (2010),  181–184
  7. Остаточные напряжения в цилиндрических образцах с V-образными надрезами из стали ВНС40 после различных видов обработки

    Matem. Mod. Kraev. Zadachi, 1 (2010),  178–181
  8. Влияние термоэкспозиции на остаточные напряжения и предел выносливости упрочнённых образцов из алюминиевых сплавов

    Matem. Mod. Kraev. Zadachi, 1 (2010),  175–177
  9. Predictions of Fatigue Endurance Limit of Hardening Samples at Elevated Temperature

    Vestn. Samar. Gos. Tekhn. Univ., Ser. Fiz.-Mat. Nauki [J. Samara State Tech. Univ., Ser. Phys. Math. Sci.], 1(20) (2010),  218–221
  10. Regularity of Auxiliary Residual Stresses Distribution into the Surface Treated Cylindrical Details with Annular Semicircular Notches

    Vestn. Samar. Gos. Tekhn. Univ., Ser. Fiz.-Mat. Nauki [J. Samara State Tech. Univ., Ser. Phys. Math. Sci.], 1(20) (2010),  121–126
  11. Сопротивление усталости упрочнeнных деталей при различной степени концентрации напряжений

    Matem. Mod. Kraev. Zadachi, 1 (2009),  126–131
  12. Выбор оптимальных режимов поверхностного упрочнения трубопроводов холодильных машин по критерию среднеинтегральных остаточных напряжений

    Matem. Mod. Kraev. Zadachi, 1 (2009),  123–126
  13. Конечно-элементное моделирование поверхностного слоя деталей, подвергаемых упрочнению методами поверхностно пластического деформирования

    Matem. Mod. Kraev. Zadachi, 1 (2009),  121–122
  14. Выбор оптимального режима пневмодробеструйной обработки по критерию среднеинтегральных остаточных напряжений

    Matem. Mod. Kraev. Zadachi, 1 (2009),  118–120
  15. Residual stresses in samples of D16T and V95 alloy after air shot peening treatment

    Vestn. Samar. Gos. Tekhn. Univ., Ser. Fiz.-Mat. Nauki [J. Samara State Tech. Univ., Ser. Phys. Math. Sci.], 2(19) (2009),  260–263
  16. A Phenomenological Approach for Modeling the Stress-strain State of Cylinder Surface Hardening Layer

    Vestn. Samar. Gos. Tekhn. Univ., Ser. Fiz.-Mat. Nauki [J. Samara State Tech. Univ., Ser. Phys. Math. Sci.], 1(18) (2009),  159–168
  17. Calculation-experimental Research of Residual Stresses Stability in Hardened Layer Of the Cylindrical Sample to Thermal Loads

    Vestn. Samar. Gos. Tekhn. Univ., Ser. Fiz.-Mat. Nauki [J. Samara State Tech. Univ., Ser. Phys. Math. Sci.], 1(18) (2009),  101–113
  18. Особенности распределения остаточных напряжений в цилиндриеских деталях после дробеструйной обработки

    Matem. Mod. Kraev. Zadachi, 1 (2008),  229–232
  19. Прогнозирование сопротивления усталости упрочнeнных деталей с различными концентраторами напряжений

    Matem. Mod. Kraev. Zadachi, 1 (2008),  143–148
  20. Релаксация остаточных напряжений в образцах с надрезами из сплавов ЭИ698ВД и ЖСУ6У

    Matem. Mod. Kraev. Zadachi, 1 (2008),  139–143
  21. Прогнозирование предела выносливости упрочнeнных деталей при различных деформациях

    Matem. Mod. Kraev. Zadachi, 1 (2008),  135–139
  22. Оптимизация режимов упрочнения маложeстких деталей ГТД

    Matem. Mod. Kraev. Zadachi, 1 (2008),  132–135
  23. Residual stresses and fatigue resistance of cylindrical volute springs

    Vestn. Samar. Gos. Tekhn. Univ., Ser. Fiz.-Mat. Nauki [J. Samara State Tech. Univ., Ser. Phys. Math. Sci.], 2(17) (2008),  254–257
  24. Влияние масштабного фактора на сопротивление усталости упрочненных деталей с концентраторами напряжений

    Matem. Mod. Kraev. Zadachi, 1 (2007),  174–177
  25. Закономерности распределения остаточных напряжений в упрочненных цилиндрических деталях с отверстием различного диаметра

    Matem. Mod. Kraev. Zadachi, 1 (2007),  171–174
  26. Остаточные напряжения и предел выносливости деталей с концентраторами напряжений при растяжении–сжатии

    Matem. Mod. Kraev. Zadachi, 1 (2007),  124–125
  27. Прогнозирование предела выносливости упрочненных деталей с концентраторами напряжений при повышенных температурах

    Matem. Mod. Kraev. Zadachi, 1 (2007),  122–123
  28. Прогнозирование предела выносливости упрочненных деталей с концентраторами напряжений при растяжении–сжатии

    Matem. Mod. Kraev. Zadachi, 1 (2006),  152–153
  29. Остаточные напряжения и предел выносливости при изгибе деталей с концентраторами напряжений

    Matem. Mod. Kraev. Zadachi, 1 (2006),  150–151